矿床地质:2017,Vol.>>Issue(1):25-37

东天山天宇铜镍硫化物矿床磁黄铁矿Re-Os同位素物质来源示踪
中国地质科学院矿产资源研究所 国土资源部成矿作用与资源评价重点实验室, 北京 100037;长安大学地球科学与资源学院, 陕西 西安 710054,中国地质科学院矿产资源研究所 国土资源部成矿作用与资源评价重点实验室, 北京 100037,中国地质科学院, 北京 100037,新疆维吾尔自治区地质矿产勘查开发局, 新疆 乌鲁木齐 830000,中国地质科学院矿产资源研究所 国土资源部成矿作用与资源评价重点实验室, 北京 100037
Re-Os isotopic analysis of pyrrhotite from Tianyu Cu-Ni sulfide deposit in Eastern Tianshan Mountains, Xinjiang: Constraints on sources of ore-forming materials
DUAN ShiGang,JIANG ZongSheng,ZHANG ZuoHeng,LI FengMing,REN YaQiong
(MLR Key Laboratory of Metallogeny and Mineral Assessment, Institute of Mineral Resources, Chinese Academy of Geological Sciences, Beijing 100037, China;College of Earth Science and Land Resources, Chang'an University, Xi'an 710054, Shaanxi, China;Xinjiang Bureau of Geology and Mineral Resources, Urumqi 830000, Xinjiang, China)
本文二维码信息
码上扫一扫!

摘要
图/表
参考文献
相似文献

摘要点击次数: 2110   全文下载次数: 2783   点此下载全文
投稿时间:2015-09-21   修订日期:2016-12-20      网络发布日期:2017-03-11
中文摘要:天宇岩浆铜镍硫化物矿床的矿体由浸染状矿体和块状矿体组成。采用同位素稀释Triton-plus测定了浸染状矿石和块状矿石的磁黄铁矿Re-Os同位素比值。结果表明:浸染状矿石w(Re)为11.82×10-9~45.28×10-9w(Os)为0.944×10-9~8.528×10-9187Os/188Os初始比值为0.885~2.332,γOs为607~1763;块状矿石w(Re)为49.38×10-9~315.10×10-9w(Os)为0.191×10-9~42.420×10-9187Os/188Os初始比值为0.654~3.322,γOs为423~2555。Re、Os含量、同位素组成和特征值表明,该矿床物质为壳-幔混合来源,块状矿石可能比浸染状矿石经历了更强的地壳物质混染。浸染状矿体发育透闪石化、蛇纹石化、绿泥石化蚀变,表明存在岩浆期后热液活动,但块状矿体热液蚀变不明显,块状矿石的Re-Os同位素特征可能是与地壳岩石直接作用的结果。地壳混染作用发生在深部岩浆房,同时也发生在岩浆侵位及再次迁移过程中,这些过程造成块状矿体与浸染状矿体不同的同位素特征。
Abstract:The Tianyu Cu-Ni sulfide deposit is composed of spatially adjacent disseminated orebody and massive orebody, with the former formed earlier than the latter. In this study, the authors used isotopic dilution Triton-plus to determine the Re-Os isotopic ratios of pyrrhotite from the disseminated ore and the massive ore. In the disseminated ore, the Re content is from 11.82×10-9 to 45.28×10-9, the Os content is from 0.944×10-9 to 8.528×10-9, the initial 187Os/188Os ratio is from 0.885 to 2.332, and γOs is from 607 to 1763. In massive ore, the Re content is from 49.38×10-9 to 315.10×10-9, the Os content is from 0.191×10-9 to 42.420×10-9, the initial 187Os/188Os ratio is from 0.654 to 3.322, and γOs is from 423 to 2555. Element content, isotopic composition and characteristic values of Re and Os indicate that the ore-forming material in the Tianyu ore deposit was a mixed source of the crust and the mantle, and the massive ore experienced a higher degree of crustal contamination than the disseminated ore. Alteration of tremolite, serpentine and chlorite is developed in the disseminated ore, which indicates post-magmatic hydrothermal activity. In contrast, the massive ore does not show obvious magmatic hydrothermal alteration. Re-Os isotopic characteristics of the massive ore might have resulted from direct interaction with crustal rocks. As a result, crustal contamination was developed both in the deep magma chamber and at the present position of the orebody.
文章编号:    
中图分类号:P597     
文献标志码:

基金项目:本文为中央科研院所基本科研业务费项目(编号:K1202)、国家自然科学基金项目(编号:41203035)和地质矿产调查评价项目(编号:1212011220894-2、1212011090300)资助成果
引用文本:
段士刚,蒋宗胜,张作衡,李凤鸣,任雅琼.2017.东天山天宇铜镍硫化物矿床磁黄铁矿Re-Os同位素物质来源示踪[J].矿床地质,36(1):25~37
DUAN ShiGang,JIANG ZongSheng,ZHANG ZuoHeng,LI FengMing,REN YaQiong.2017.Re-Os isotopic analysis of pyrrhotite from Tianyu Cu-Ni sulfide deposit in Eastern Tianshan Mountains, Xinjiang: Constraints on sources of ore-forming materials[J].Mineral Deposits36(1):25~37
图/表
您是第242455752位访问者  京ICP备05032737号-5  京公网 安备110102004559
主管单位:中国科学技术协会 主办单位:中国地质学会矿床地质专业委员会 中国地质科学院矿产资源研究所
地  址: 北京市百万庄大街26号 邮编:100037 电话:010-68327284;010-68999546 E-mail: minerald@vip.163.com
本系统由北京勤云科技发展有限公司设计 
手机扫一扫